Short Lead Time for Ptfe Vacuum Tubing - PTFE Heat Resistant Tube Tubing Pipe | BESTEFLON – Besteflon
Short Lead Time for Ptfe Vacuum Tubing - PTFE Heat Resistant Tube Tubing Pipe | BESTEFLON – Besteflon Detail:
Product Details
| Brand Name: | BESTEFLON |
| Color: | Milky white / translucent / black / blue / red / orange and etc. |
| Specification: | 2x4mm, 4x6mm, 6x8mm, 8x10mm, 10x12mm, 12x14mm, 16x18mm and etc. |
| Thickness: | 1mm, 1.5mm, 2mm, or custom thickness |
| Material: | 100% virgin PTFE |
| Working Temperature Range: | -65℃-+260℃ |
| Application: | 3D Printer, chemical transfer, high purity fluids transfer, air sampling, and etc. |
| Business Type: |
Manufacturer/Factory |
| Standard: | ISO9001, FDA, RoHS, and etc. |
Smooth Bore Tubing Imperial Range
| No. | Specification | Outer diameter | Inner diameter | Tube Wall Thickness | Working pressure | Burst pressure | |||||
| mm | (inch) | mm | (inch) | mm | (inch) | (psi) | (bar) | (psi) | (bar) | ||
| 1 | 1/8″*1/16″ | 3.17 | 0.125 | 1.58 | 0.062 | 0.8 | 0.031 | 218 | 15.0 | 725 | 50 |
| 2 | 3/16″*1/8″ | 4.76 | 0.187 | 3.17 | 0.125 | 0.8 | 0.031 | 174 | 12.0 | 638 | 40 |
| 3 | 1/4″*3/16″ | 6.35 | 0.250 | 4.76 | 0.187 | 0.8 | 0.031 | 131 | 9.0 | 464 | 32 |
| 4 | 5/16″*1/4″ | 7.93 | 0.312 | 6.35 | 0.250 | 0.8 | 0.031 | 102 | 7.0 | 363 | 25 |
| 5 | 3/8″*1/4″ | 9.52 | 0.357 | 6.35 | 0.250 | 1.5 | 0.059 | 174 | 12.0 | 638 | 44 |
| 6 | 3/8″*5/16″ | 9.52 | 0.357 | 7.93 | 0.312 | 0.8 | 0.031 | 87 | 6.0 | 319 | 22 |
| 7 | 1/2″*3/8″ | 12.7 | 0.500 | 9.6 | 0.378 | 1.5 | 0.059 | 131 | 9.0 | 464 | 32 |
| 8 | 5/8″*1/2″ | 15.87 | 0.625 | 12.7 | 0.500 | 1.5 | 0.059 | 102 | 7.0 | 363 | 25 |
| 9 | 3/4″*5/8″ | 19.05 | 0.750 | 15.87 | 0.625 | 1.5 | 0.059 | 87 | 6.0 | 319 | 22 |
* Customer-specific products may be discussed with us for detailed.
Smooth Bore Tubing Metric Range
| No. | Specification | Outer diameter | Inner diameter | Tube Wall Thickness | Working pressure | Burst pressure | |||||
| mm | (inch) | mm | (inch) | mm | (inch) | (psi) | (bar) | (psi) | (bar) | ||
| 1 | 2*4 | 4 | 0157 | 2 | 0.079 | 1 | 0.039 | 148 | 10.2 | 444 | 30.6 |
| 2 | 3*5 | 5 | 0.197 | 3 | 0.118 | 1 | 0.039 | 148 | 10.2 | 444 | 30.6 |
| 3 | 4*6 | 6 | 0.236 | 4 | 0.157 | 1 | 0.039 | 148 | 10.2 | 444 | 30.6 |
| 4 | 5*7 | 7 | 0.276 | 5 | 0.197 | 1 | 0.039 | 148 | 10.2 | 444 | 30.6 |
| 5 | 6*8 | 8 | 0.315 | 6 | 0.236 | 1 | 0.039 | 148 | 10.2 | 444 | 30.6 |
| 6 | 8*10 | 10 | 0.394 | 8 | 0.315 | 1 | 0.039 | 148 | 10.2 | 444 | 30.6 |
| 7 | 10*12 | 12 | 0.472 | 10 | 0.394 | 1 | 0.039 | 118 | 8.16 | 370 | 25.5 |
| 8 | 12*14 | 14 | 0.551 | 12 | 0.472 | 1 | 0.039 | 118 | 8.16 | 370 | 25.5 |
| 9 | 14*16 | 16 | 0.630 | 14 | 0.551 | 1 | 0.039 | 118 | 8.16 | 370 | 25.5 |
| 10 | 16*18 | 18 | 0.709 | 16 | 0.630 | 1 | 0.039 | 118 | 8.16 | 370 | 25.5 |
| 11 | 20*24 | 24 | 0.945 | 20 | 0.787 | 2 | 0.079 | 74 | 5.1 | 296 | 20.4 |
| 12 | 50*54 | 54 | 2.126 | 50 | 1.969 | 2 | 0.079 | 74 | 5.1 | 296 | 20.4 |
Learn more about BESTEFLON products
People also ask
2.How to Remove Stuck Filament from PTFE Tube
3.Fkm rubber vs ptfe: which is the ultimate fluorinated material
Video
Give Us A E-Mail
sales02@zx-ptfe.com
Product detail pictures:
Related Product Guide:
Our rewards are lower costs,dynamic profits team,specialised QC,potent factories,high-quality services for Short Lead Time for Ptfe Vacuum Tubing - PTFE Heat Resistant Tube Tubing Pipe | BESTEFLON – Besteflon , The product will supply to all over the world, such as: San Diego, Gambia, Hungary, We confirm to public, cooperation, win-win situation as our principle, adhere to the philosophy of make a living by quality, keep developing by honesty , sincerely hope to build up a good relationship with more and more customers and friends, to achieve a win-win situation and common prosperity.
We offer the usual packing as follows
1、Nylon bag or poly bag
2、Carton box
3、Plastic pallet or plywood pallet
Customized Packaging is charged
1、Wooden reel
2、Wooden case
3、Other customized packaging also available
As a veteran of this industry, we can say that the company can be a leader in the industry, select them is right.
Send your message to us: